Detailed sample fabrication and characterization procedure, XRR best-fit results, TEM sublayer intensity variation profiles, different frequency response regimes of σ_ac profiles, measured and deconvo
The supplementary material provides additional data and supporting analyses to complement the findings presented in the article.FIG.S1. shows the test results of the collision parameters.Table S1 and