XRD patterns of nickel-modified V2CTx
收藏数据链接:
官方服务:
资源简介:
The set includes data for XRD pattern preparation of nickel-modified V2CTx samples. Preparation of V2CTx: V2AlC was subjected to selective removing of aluminium via etching in 50% HF at room temperature for 96 h. Preparation of Ni-V2CTx_NaOH: hydrothermal synthesis of nickel particles deposition on V2CTx MXene in basic media (pH=10) at 160 deg. C. for 16h
创建时间:
2021-07-14