Kikuchi pattern dataset from wrought and as-built additively manufactured superalloys

收藏
DataCite Commons2026-01-29 更新2026-04-25 收录
官方服务:

资源简介:

This dataset provides high-resolution Kikuchi diffraction patterns and associated orientation mapping data collected from both wrought and as-built additively manufactured (AM) Inconel 718 superalloys. The dataset includes raw electron backscatter diffraction (EBSD) patterns stored as .tif images and organized through .up2 metadata files, along with processed orientation data in .ang format. These measurements were acquired using a high-sensitivity EBSD detector over large scan areas, enabling detailed spatial resolution of microstructural features such as grain orientations, subgrain boundaries, and processing-induced texture. The dataset supports a range of applications, including machine learning for pattern recognition and the development of robust indexing algorithms. By including both wrought and AM material states, this dataset offers valuable insight into the influence of manufacturing route on crystallographic texture and cellular dislocation structure in Inconel 718, a critical alloy for high-temperature structural applications.

提供机构:
Dryad
创建时间:
2025-09-16
二维码
社区交流群
二维码
科研交流群
商业服务