遇见数据集

Small punch creep test data for AISI 316L ar material at 600 °C and a load of 500 N (specimen identifier FK-15)

收藏
DataCite Commons2024-10-31 更新2025-04-16 收录
官方服务:

资源简介:

Data created at JRC, Netherlands during the Horizon 2020 NUCOBAM project aiming to develop the qualification process and evaluate the in-service behaviour of AM materials, allowing the use of additively manufactured components in nuclear installations. The project has received funding from the Euratom research and training programme 2014-2018 under Grant Agreement No. 945313.

创建时间:
2024-10-31
二维码
社区交流群
二维码
科研交流群
商业服务