Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.002 mN (thirty-ninth nominally repeat test)
收藏DataCite Commons2020-10-05 更新2025-05-18 收录
下载链接:
https://odin.jrc.ec.europa.eu/alcor/DOIDisplay.html?p_RN5=1200131
下载链接
链接失效反馈官方服务:
资源简介:
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.
创建时间:
2020-01-07